Fifteen different lithium-hydroxyapatite composites were tested in this work. LiHA were prepared using 0.25 %, 1 % and 2 % of lithium and five different sintering temperature 900, 1000, 1100, 1200 and 1300oC. Primary culture of osteoblasts were used to evaluate the biocompatibility of the samples, concerning to cell viability and alkaline phosphatase production. The 1% LiHA samples sintered at 1100, 1200 and 13000C showed the best results.

信息:

期刊:

主题:

编辑:

Takashi Nakamura, Kimihiro Yamashita and Masashi Neo

页数:

1121-1124

DOI:

10.4028/www.scientific.net/KEM.309-311.1121

引用:

P. Valério et al., "Biocompatibility Evaluation of Lithium-Hydroxyapatite Composites", Key Engineering Materials, Vols. 309-311, pp. 1121-1124, 2006

上线时间:

May 2006

输出:

价格:

$35.00

[1] L L Hench Bioceramics. J Am Ceram Soc. Vol 74 (1991), p.1487.

[2] R Z Legeros. An introduction to bioceramics L. L. Hench. World Scientific Publication Singapure (1993).

[3] J W Choi et al.: J. Am. Ceram. Soc. Vol 81 (1998), p.1743.

[4] I Mayer et al.: Calcif. Tissue Int. Vol 38 (1986), pp.293-5.

[5] SH Oh: J. Biomed Mater. Res. Vol 67A (2003), pp.104-11.

[6] G Goller et al.: Key Engineering Materials. Vol 240-242 (2003).

为了查看相关信息, 需 Login.