Microstructure Characteristics of the Reaction Product Region Formed due to the High Temperature Contact of Molten Aluminium and ZnO Single Crystal

摘要:

文章预览

Interface reactions between liquid aluminium and ZnO single crystal substrates of <1-100> orientation (at 1273 K under vacuum) were examined using scanning and transmission electron microscopy techniques. The substrates were subjected to the “pushing drop” tests when liquid is deposited from the capillary on the substrate surface and then, after appropriate contact time, it is pushed away. After short time of interaction with <1-100>ZnO substrate, three phases were detected: α-Al2O3, the alumina of unknown type and ZnAl2O4 spinel formed due to the solid state reaction between Al2O3 and ZnO.

信息:

期刊:

Solid State Phenomena (172-174卷)

编辑:

Yves Bréchet, Emmanuel Clouet, Alexis Deschamps, Alphonse Finel and Frédéric Soisson

页数:

1267-1272

DOI:

10.4028/www.scientific.net/SSP.172-174.1267

引用:

J. Wojewoda-Budka et al., "Microstructure Characteristics of the Reaction Product Region Formed due to the High Temperature Contact of Molten Aluminium and ZnO Single Crystal", Solid State Phenomena, Vols. 172-174, pp. 1267-1272, 2011

上线时间:

June 2011

输出:

价格:

$35.00

[1] N. Sobczak: Solid State Phenomena Vol. 101-102 (2005), p.221.

[2] T.W. Clyne and P.J. Withers: An Introduction to Metal Matrix Composites (Cambridge, UK 1995).

[3] M. C. Breslin, J. Ringnalda, L. Xu, M. Fuler, J. Seeger, G. S. Daehn, T. Otani and H.L. Fraser: Mat Sci Eng A Vol. 195 (1995), p.113.

[4] W. Liu and U. Koster: Script. Mater. Vol. 35 (1996), p.35.

[5] American Society for Metals Handbook, 1973, p.265, Metals Park, OH.

[6] M. Kobasi and T. Choh: Light Met. 42 (1992), p.138.

[7] G. Chen and G.X. Sun: Materials Science and Engineering A244 (1998), p.291.

[8] T.G. Durai, K. Das and S. Das: Materials Science and Engineering A 445–446 (2007), p.100.

[9] Y. Peng: Mater. Lett. Vol. 58 (2004), p.679.

[10] N. Sobczak, A. Kudyba, R. Nowak, W. Radziwill and J. Oblakowski: Ceramika/Ceramics (Polish Ceramic Bulletin) Vol. 80 (2005), p.661.

[11] J. Wojewoda-Budka, N. Sobczak, J. Morgiel and R. Nowak: J. Mater. Sci. Vol. 45(16) (2010) p.4291.

DOI: 10.1007/s10853-010-4379-6

[12] J. Wojewoda-Budka, N. Sobczak, J. Morgiel and R. Nowak: Archives of Metallurgy (2010), in print.

[13] N. Sobczak, in: Innovations in Foundry Part II, edtied by J. Sobczak, Foundry Research Institute, Krakow, Poland (2007).

[14] P. Shen, H. Fujii, T. Matsumoto and K. Nogi: Acta Materialia Vol. 52 (2004), p.887.

[15] M. Ay, A. Nefedov, S. Gil Girol, Ch. Wöll, H. Zabel: Thin Solid Films Vol. 510 (2006), p.346.

DOI: 10.1016/j.tsf.2005.12.271

[16] S.H. Lima, D. Shindo, H.B. Kang, K. Nakamura: Journal of Crystal Growth Vol. 225 (2001), p.202.

[17] S. Pin, P. Ghigna, G. Spinolo, E. Quartarone, P. Mustarelli, F. D'Capito, A. Migliori, G. Calestani: J. Solid State Chem. Vol. 182 (2009), p.1291.

DOI: 10.1016/j.jssc.2009.02.027

为了查看相关信息, 需 Login.