Deformation of Ti-6Al-4V Alloy with Carbon

摘要:

文章预览

This paper presents the results from investigations on the effect of temperature and strain rate on the shape of the stress-strain curves, the peak flow stress and microstructure of Ti-6Al-4V alloy with carbon (0.7–0.8 wt%) that were axisymmetrically compressed on a thermo-mechanical simulator Gleeble 3800. Conditions under which the alloy deformation proceeded without cracking were determined. The obtained results were verified by industrial open die forging tests.

信息:

期刊:

编辑:

Agnieszka Botor-Probierz and Andrzej Kiełbus

页数:

149-156

DOI:

10.4028/www.scientific.net/SSP.176.149

引用:

A. Szkliniarz "Deformation of Ti-6Al-4V Alloy with Carbon", Solid State Phenomena, Vol. 176, pp. 149-156, 2011

上线时间:

June 2011

输出:

价格:

$35.00

[1] I.V. Gorynin and N.F. Anoshkin: State of Production and Application of Titanium in the CIS. Ti-2003 Science and Technology, WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim (2004).

[2] H.R. Ogden and R I. Jaffee: Titanium Metallurgical Laboratory Report No. 20, Ohio (1955).

[3] O.P. Solonina and N.M. Ulyakova: Mater. Sci. and Heat Treat. Vol. 16 (1974), p.310.

[4] J. Grauman, S. Fox, and S. Nyakana, U.S. Patent US 2006/035867. (2006).

[5] S. Kojima and H. Oyama, U.S. Patent US 2003/0098099A1. (2003).

[6] Y.G. Li and P.A. Blenkinsop, U.S. Patent US 2006/0021680A1. (2006).

[7] X. Wu, M.Q. Chu and I. Jones, U.K. Patent GB 2423089A. (2005).

[8] H. Kashii, A. Nakamura, N. Kitazaki, Y. Kitagawa and K. Koine, U.S. Patent US 5759484. (1998).

[9] R. Jaffee, H. Ogden and D. Maykuth, U.S. Patent US 2669513 A1. (1954).

[10] B.A. Kolachev, A.V. Malkov and V.I. Sedov: Mater. Sci. and Heat Treat. Vol. 17 (1975), p.226.

[11] Z.Q. Chen, Y.G. Li, M.H. Loretto and X. Wu: Mater. Sci. and Tech., Vol. 19 (2003), p.1391.

为了查看相关信息, 需 Login.